SAMBUNGAN BALOK BETON BERTULANG PRACETAK DENGAN LAPISAN CARBON FIBER REINFORCED POLYMER DAN PLAT BAJA

Conceição, Gilberto De Carvalho Da (2019) SAMBUNGAN BALOK BETON BERTULANG PRACETAK DENGAN LAPISAN CARBON FIBER REINFORCED POLYMER DAN PLAT BAJA. S2 thesis, uajy.

[img]
Preview
Text (HALAMAN AWAL)
1651026050.pdf

Download (1MB) | Preview
[img]
Preview
Text (BAB I)
1651026051.pdf

Download (149kB) | Preview
[img]
Preview
Text (BAB II)
1651026052.pdf

Download (236kB) | Preview
[img] Text (BAB III)
1651026053.pdf
Restricted to Registered users only

Download (578kB)
[img] Text (BAB IV)
1651026054.pdf
Restricted to Registered users only

Download (1MB)
[img] Text (BAB V)
1651026055.pdf
Restricted to Registered users only

Download (994kB)
[img]
Preview
Text (BAB VI)
1651026056.pdf

Download (2MB) | Preview

Abstract

Precast reinforced concrete beams are building structures without using on-site casting and can shorten Construction time, and reduce costs and labor. But as for the shortcomings of this method, the precision (precision) in concrete printing, the strength of the precast concrete connection system itself. Apart from also because of its large segment, it is not easy to carry out transportation, erection, and lifting. In this research a method was used to overcome the shortcomings of the precast method in terms of weight and size, by dividing the precast segment into a new connection between the beam to the beam where the connection was reinforced with Carbon Fiber Reinforced Contrete and steel plate. Where there are 2 beam joints namely Type II connection on the connection area, steel plate and bolt data are used as Type III washers and joints, CFRP is added to the joint area and 6 mm thick steel plate and 20 mm diameter bolt. The dimensions of the beams used are 150 x 250 x 3200 mm with 4P10 longitudinal reinforcement as pressure reinforcement and 2P10 as pressure reinforcement. While 2P8-200 as shear reinforcement in the field area, 2P8-150 for Sammbungan area and 2P8-100 for support area. Where the quality of reinforcing steel in this method is BjTP 24, with a yield stress of 323.533 MPa for P10 and 237,249 MPa for P8. According to the results of the study the beam joints with centralized loading, the type II joint beam obtained a load capacity of 2782,718 kg while the type III connection experienced a load increase of 3553,875 kg due to the addition of CFRP layers on the beam joints.

Item Type: Thesis (S2)
Uncontrolled Keywords: s: precast concrete, beam joint, CFRP, flexural capacity
Subjects: Magister Teknik Sipil > Struktur
Divisions: Pasca Sarjana > Magister Teknik Sipil
Depositing User: wiwid bartolomeus wijayanto
Date Deposited: 16 Sep 2019 05:13
Last Modified: 16 Sep 2019 05:13
URI: http://e-journal.uajy.ac.id/id/eprint/19980

Actions (login required)

View Item View Item